Chemical Composition of steel bar
Category | Steel bar remark | Chemical composition (%) | |||||
C | Mn | P | S | Si | C.E. | ||
CNS 560 |
SD 280 W (hot rolled) | 0.30 max | 1.50 max | 0.040 max | 0.040 max | 0.50 max | 0.55 max |
SD 420 W (hot rolled) | 0.30 max | 1.50 max | 0.040 max | 0.040 max | 0.50 max | 0.55 max | |
SD 280 W (heat treatment) | 0.22 max | 1.60 max | 0.040 max | 0.040 max | 0.60 max | 0.50 max | |
SD 420 W (heat treatment) | 0.22 max | 1.60 max | 0.040 max | 0.040 max | 0.60 max | 0.50 max |
Chemical Composition of steel bar
CNS | |||||||
Steel bar remark | Yield strength (Y.S)N/ mm | Tensile Strength (T.S)N/ mm | Tensile strength / Yield strength | Test fragment | Elongation(%) | Solidworks | |
angle | diamete | ||||||
CNS 560 | 280 min | 420 min | - | NO.2 | 14 min | 180 | 4D |
NO. 14A | 17 min | ||||||
SD 280 W | 280 ~ 380 min | 420 min | 1.25 min | NO. 2 | 14 min | 180 | 4D |
NO. 14A | 17 min | ||||||
SD 420 W | 420 ~ 540 min | 550 min | 1.25 min | NO. 2 | 12 min | 180 | D10-D16 3D D19-D25 4D Over D25 6D |
Product to be use for Steel bar
Building construction, Tunnel construction and Bridge building